A research team has demonstrated that systematically adjusting the concentration of ammonium chloride additive in an electrochemical deposition bath allows precise control over the elemental composition, atomic-scale coordination, and catalytic performance of amorphous nickel-phosphorus alloy coatings designed for the hydrogen evolution reaction. Water splitting via alkaline water electrolysis represents an established commercial approach to producing green hydrogen carrier fuel from renewable resources, yet standard nickel-based electrodes frequently suffer from operational passivation and corrosive degradation over extended operational periods. To resolve these operational limitations, investigators synthesized three distinct nickel-phosphorus thin-film coatings on copper foil substrates using pulsed electrodeposition, varying solely the molar concentration of ammonium chloride within the electrolyte bath across three designated levels of 0.2 M, 1 M, and 3 M. Comprehensive material and electrochemical characterization revealed that higher additive concentrations produced smoother surface textures, reduced the average nickel-to-phosphorus ratio from 6.2 to 4.7, increased the local coordination number of nickel to phosphorus from 0.5 to 0.9, and lowered the catalytic Tafel slope to 53.9 millivolts per decade in alkaline electrolyte.
Green hydrogen serves as a clean, sustainable energy carrier possessing an estimated calorific energy value of approximately 142 megajoules per kilogram, which can be extracted from water through various electrochemical, thermochemical, photoelectrochemical, and photocatalytic techniques. Although alkaline water electrolysis currently maintains operational industrial units capable of coupling directly with renewable power sources such as wind and solar installations, the process remains less cost-effective overall than conventional steam methane reforming. Improving the inherent half-cell kinetics of both the oxygen evolution reaction at the anode and the hydrogen evolution reaction at the cathode is therefore crucial for elevating overall electrolyzer efficiency. Metallic nickel surfaces represent standard catalytic materials in alkaline media, but their vulnerability to surface passivation during sustained electrolysis has driven extensive scientific exploration into binary nickel alloys containing molybdenum, copper, iron, cobalt, tungsten, or phosphorus to stabilize reaction interfaces and accelerate hydrogen generation.
Among transition metal binary systems, nickel-phosphorus alloy coatings have attracted substantial investigation due to their robust catalytic stability, low raw material expense, elemental abundance, and favorable electrochemical attributes. Prior scientific inquiries have established that the crystalline nature and elemental phosphorus concentration of nickel-phosphorus deposits significantly govern their ultimate hydrogen evolution reaction activity. Depending on synthesis parameters, both crystalline and amorphous structures can be obtained, with amorphous phases frequently exhibiting enhanced hydrogen absorption and internal stress that facilitate catalytic hydrogen generation. However, literature reports have historically presented conflicting conclusions regarding optimal phosphorus loading, with independent studies identifying peak performance at 7 weight percent phosphorus, 10 weight percent phosphorus, or reporting generalized activity declines as phosphorus content escalated. Furthermore, earlier electrodeposition methodologies generally lacked an integrated mechanistic framework connecting additive-driven electrolyte bath chemistry directly to deposit stoichiometry, local atomic coordination, and resulting alkaline half-cell kinetics.
To establish a systematic relationship between bath additive chemistry and catalytic behavior, the experimental study employed a pulsed electrodeposition methodology utilizing a three-electrode glass cell setup. Working electrodes consisted of 0.2-millimeter-thick copper foils featuring an exposed working area of two square centimeters, paired against a graphite counter electrode and a silver-silver chloride reference electrode. Pre-deposition surface preparation of the copper substrates involved manual polishing with abrasive emery paper, ultrasonic cleaning in a 1 M hydrochloric acid solution for five minutes, sequential rinsing with nanopure distilled water and acetone, and thorough air drying to achieve a consistent finish. The baseline electroplating electrolyte was formulated with analytical-grade nickel chloride hexahydrate and sodium hypophosphite hexahydrate dissolved in nanopure water, into which ammonium chloride was introduced at concentrations of 0.2 M, 1 M, or 3 M to generate samples designated respectively as NP02, NP1, and NP3. Continuous magnetic stirring and inert nitrogen gas purging were maintained throughout the process, while cathodic pulse electrodeposition was conducted over 100,000 cycles using a rectangular waveform comprising a 20-milliampere pulse for 1 millisecond followed by a zero-current off interval of 9 milliseconds.
Structural evaluation of the synthesized alloy coatings via powder X-ray diffraction, conducted with copper K-alpha radiation at 40 kilovolts and 30 milliamperes, confirmed the non-crystalline character of all three electrodeposited films. The resulting diffraction profiles exhibited diffraction reflections corresponding exclusively to the underlying cubic metallic copper substrate, with no identifiable diffraction peaks associated with crystalline nickel phases, confirming that pulsed electrodeposition produced fully amorphous alloy coatings. Examination of three-dimensional surface topographies through contact-mode atomic force microscopy using silicon nitride tips revealed marked differences in surface roughness directly attributable to additive bath concentration. The NP02 coating synthesized with 0.2 M ammonium chloride exhibited an irregular surface topography dominated by tall, sharp protrusions indicative of rapid, non-uniform nucleation and growth kinetics. Conversely, advancing to the NP1 and NP3 specimens revealed a progressive smoothening of surface features, accompanied by a systematic reduction in vertical protrusions and the formation of well-distributed, shallow surface pores indicative of slower, more homogeneous film accretion.
Microstructural observations gathered through field emission scanning electron microscopy operating at an accelerating voltage of 5 kilovolts corroborated the structural transformations recorded by atomic force imaging. Micrographs of the NP02 sample revealed a compact surface layer interrupted by sporadic granules and distorted spheroidal particles measuring between 100 and 200 nanometers across, along with visible network microcracks. These microcracks represent release pathways for tensile mechanical stresses generated by localized hydrogen evolution occurring as a secondary reaction during cathodic electrodeposition. In contrast, the NP1 coating demonstrated a compact, crack-free morphology containing much smaller, uniformly dispersed particulate grains ranging from 20 to 50 nanometers in diameter alongside occasional larger agglomerates. The NP3 deposit, synthesized at the highest additive loading of 3 M, exhibited a highly uniform, compact surface completely populated with fine irregular nodules and small 20-to-50-nanometer particulates. Cross-sectional electron microscopy measurements across the NP02 and NP3 coatings indicated consistent overall film thicknesses measuring between 1.6 and 1.7 micrometers.
Compositional quantification performed through energy-dispersive X-ray spectroscopy across four distinct localized surface regions per specimen demonstrated a direct correlation between bath additive levels and alloy stoichiometry. The average nickel-to-phosphorus elemental ratio exhibited an orderly, monotonic decline as the ammonium chloride concentration was elevated, decreasing from approximately 6.2 in NP02 to intermediate values in NP1, and down to approximately 4.7 in the NP3 coating. Energy-dispersive X-ray fluorescence maps collected under low magnification over broader surface areas revealed that spatial deviations in nickel and phosphorus concentrations were most pronounced in the low-additive NP02 sample and lowest in the high-additive NP3 coating. Raising the ammonium chloride content in the electrochemical bath therefore systematically boosted the relative phosphorus incorporation while ensuring a more spatially homogeneous elemental distribution across the entire electrodeposited copper surface.
Synchrotron-based X-ray absorption spectroscopy conducted at the Scanning EXAFS Beamline BL-9 of the Indus-2 Synchrotron Source at the Raja Ramanna Centre for Advanced Technology in Indore, India, elucidated the local coordination environments of the alloys. Measurements performed at the nickel K-edge in fluorescence mode using a silicon drift detector showed that the absorption edge position for all three amorphous coatings aligned with that of metallic nickel foil, confirming that nickel atoms existed predominantly in a metallic zero-valent oxidation state. Quantitative fitting of extended X-ray absorption fine structure radial distribution functions over a k-range of 2.5 to 9 inverse angstroms resolved a nickel-nickel bonding shell between 2.45 and 2.49 angstroms, closely matching interatomic distances in polycrystalline nickel foil. In addition, an interstitial nickel-phosphorus coordination shell was resolved at shorter interatomic distances ranging from 2.17 to 2.19 angstroms. Crucially, mathematical structural refinement revealed that the coordination number of nickel with adjacent phosphorus atoms progressively increased from 0.5 in NP02 to 0.9 in NP3, proving that phosphorus incorporation increasingly disrupts long-range metallic order to stabilize a short-range amorphous solid solution.
To elucidate the electrochemical mechanisms governing these structural and compositional shifts, in-situ ultraviolet-visible spectroelectrochemical experiments were carried out using a specialized one-millimeter path-length cell equipped with a platinum gauze working electrode under a constant chronoamperometric potential of minus 1.0 volt versus silver-silver chloride. In the 0.2 M bath condition of NP02, optical absorption spectra were dominated by a prominent absorbance band situated near 360 nanometers, attributed to solvated nickel ionic complexes. Under the 3 M condition of NP3, the principal optical absorption shifted decisively to approximately 208 nanometers, reflecting a spectral signature associated with concentrated ammonium chemical species. These optical observations demonstrated that elevated concentrations of ammonium cations fundamentally alter the electrical double-layer structure at the cathode interface during electrodeposition, effectively displacing nickel cations from the immediate electrode boundary layer through competitive electrostatic accumulation.
During cathodic electrodeposition, metallic nickel deposits via a two-electron reduction pathway while oxygen evolves at the counter electrode. Phosphorus cannot deposit independently from hypophosphite anions without co-deposition alongside nickel, proceeding either through direct proton-mediated reduction or via a four-electron intermediate mechanism generating adsorbed atomic hydrogen and phosphine intermediates that subsequently react with nickel cations. Concurrently, competitive reduction of ammonium cations generates adsorbed hydrogen atoms and ammonia gas at the cathode surface. As the concentration of ammonium chloride is increased from 0.2 M to 3 M, the heightened presence of competing ammonium cations diminishes localized nickel cation aggregation at the cathode double layer while simultaneously boosting the local availability of reactive adsorbed hydrogen species. Because current pulsing repeatedly dismantles and rebuilds the electrical double layer during every off-time interval, this competitive dynamic suppresses uneven nickel crystal growth, minimizes localized particle agglomeration, and facilitates multi-electron phosphorus co-deposition pathways, thereby yielding smaller, more evenly distributed alloy grains enriched in phosphorus.
Electrochemical assessment of catalytic performance toward the alkaline hydrogen evolution reaction was carried out in a 1 M potassium hydroxide electrolyte utilizing a Biologic VSP-2 workstation configured with a mercury-mercuric oxide reference electrode and a graphite counter rod. Cyclic voltammetry profiles recorded across all samples at a scan rate of 100 millivolts per second displayed an initial anodic peak near 0.7 volts versus the reversible hydrogen electrode, corresponding to the alpha-to-beta phase transition of nickel hydroxide surface layers, followed by a nickel oxidation peak at approximately 1.5 volts preceding oxygen evolution. Cathodic linear sweep voltammetry demonstrated an unambiguous enhancement in catalytic activity following the sequence NP02, NP1, and NP3. The overpotential required to achieve an operational cathodic current density of minus 10 milliamperes per square centimeter decreased consistently with higher additive content, while corresponding Tafel slopes derived from polarization curves dropped from 70.1 millivolts per decade for NP02, down to 61.3 millivolts per decade for NP1, and reaching an optimal 53.9 millivolts per decade for NP3.
Electrochemical impedance spectroscopy measurements recorded at an overpotential of 0.5 volts in 1 M potassium hydroxide further substantiated the catalytic kinetics observed in polarization curves. Nyquist impedance spectra matched a standard equivalent Randles circuit model, demonstrating that charge transfer resistance across the electrode-electrolyte interface decreased monotonically from NP02 to NP3 as the ammonium chloride concentration in the synthesis bath rose. The combined experimental findings verify that altering additive concentration during pulsed electrodeposition offers a facile, highly reproducible synthetic lever to tailor the elemental ratio, surface morphology, and short-range coordination environment of amorphous nickel-phosphorus catalysts. By concurrently refining particle dimensions, improving compositional homogeneity, and elevating the local nickel-phosphorus coordination number, this additive-mediated synthesis strategy significantly lowers overpotential barriers and accelerates alkaline hydrogen evolution kinetics without requiring complex metallurgical processing or noble metal incorporation.
Subject of Research: Electrochemical synthesis and hydrogen evolution performance of pulsed electrodeposited nickel-phosphorus alloy coatings regulated by ammonium chloride additive concentration
Article Title: Synthesis of Ni-P alloy coatings by pulsed electrodeposition: the effect of additive content on morphology, local structure and electrochemical properties for HER
Article References: Gaikwad, A. P., Tripathi, V. M., Nayak, C., Bairwa, K. K., Tripathi, V. S., Pai, M. R., & Banerjee, A. M. (2026). Synthesis of Ni-P alloy coatings by pulsed electrodeposition: the effect of additive content on morphology, local structure and electrochemical properties for HER. Materials for Renewable and Sustainable Energy, 15(1), Article 22. https://doi.org/10.1007/s40243-026-00355-9
Image Credits: AI Generated
DOI: 10.1007/s40243-026-00355-9
Keywords: nickel-phosphorus alloy, pulsed electrodeposition, hydrogen evolution reaction, alkaline water electrolysis, ammonium chloride additive, electrocatalysis, amorphous coatings, extended X-ray absorption fine structure, X-ray absorption near edge structure, Tafel slope, charge transfer resistance, in-situ spectroelectrochemistry, scanning electron microscopy, atomic force microscopy, synchrotron XAS, coordination number, green hydrogen